MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP15 High Tensile Strength One Component Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Go-to” material for use in ASTM C633 testing applications
  • Exceptionally high tensile strength
  • Excellent dimensional stability
  • Low shrinkage upon cure
Product Description: Master Bond Polymer System EP15 is a one component, heat curing epoxy featuring high tensile strength utilized in testing the adhesion and/or cohesive strength of flame sprayed coatings. This standard test is fully detailed in ASTM specification C633. EP15 is formulated to cure at temperatures from 300-350°F for 60-90 minutes. Upon cure, EP15 has a tensile strength well in excess of 12,000 psi. EP15 forms rigid and dimensionally stable bonds with minimal shrinkage upon cure. It is 100% reactive and does not contain any solvents or diluents. Its service temperature range is -60°F to +250°F. As a one component epoxy, Master Bond Polymer System EP15 is easy to handle as it does not require mixing prior to use and has an unlimited working life at room temperature. It bonds well to a wide variety of substrates, but most pertinent is its exceptionally good adhesion to metals and ceramics especially those that are flame-sprayed. The standard color of the epoxy is tan. Although primarily used in the flame sprayed coating test, EP15 can also be utilized in any bonding application where high tensile strength is a prerequisite. It is generally accepted that the liquid version of the epoxy is preferable when dealing with ceramic substrates while the paste version, called EP15ND-2, is preferable for metallic substrates.

Product Advantages:

  • Single component system; no mixing prior to use
  • Unlimited working life at room temperature
  • Easy application; contact pressure only required during heat cure
  • Exceptionally high tensile strength well exceeding 12,000 psi
  • 100% reactive; contains no solvents or volatiles
  • Bonds well to a wide range of substrates, especially flame-sprayed coatings
  • Very low shrinkage upon cure
  • Excellent dimensional stability
  • Specifically designed for testing under ASTM specification C633

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/cc
Solids Content 100 %100 %
Viscosity 40000 - 65000 cP40000 - 65000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 82.7 MPa>= 12000 psi
Adhesive Bond Strength >= 20.7 MPa>= 3000 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 90.0 min
@Temperature 149 - 177 °C
1.00 - 1.50 hour
@Temperature 300 - 350 °F
Shelf Life 3.00 - 6.00 Month
@Temperature <=23.9 °C
3.00 - 6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP101HTX-3 One Component Thermally Stable Epoxy System
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting
Master Bond EP110F6 Thermal Shock Resistant, Electrically Insulating Epoxy
Wingate Alloys Winco TGP Turned, Ground and Polished Heat-Treated High Tensile Alloy Steel
Wingate Alloys Winco Heat Treated, High Tensile Alloy Steel for Maintenance and Machine Repair

PMASTM807 / 185400

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.