MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnite® TM4 440 (PBT+PET)-MD20
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET, Mineral Filled

Material Notes: 20% Mineral Reinforced

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption 0.35 %0.35 %Sim. To ISO 62
Moisture Absorption 0.150 %0.150 %Sim. To ISO 62
Viscosity  17500 cP
@Shear Rate 100000 1/s,
Temperature 280 °C
17500 cP
@Shear Rate 100000 1/s,
Temperature 536 °F
 20000 cP
@Shear Rate 100000 1/s,
Temperature 250 °C
20000 cP
@Shear Rate 100000 1/s,
Temperature 482 °F
 25000 cP
@Shear Rate 100000 1/s,
Temperature 230 °C
25000 cP
@Shear Rate 100000 1/s,
Temperature 446 °F
 200000 cP
@Shear Rate 1 1/s,
Temperature 280 °C
200000 cP
@Shear Rate 1 1/s,
Temperature 536 °F
 500000 cP
@Shear Rate 1 1/s,
Temperature 250 °C
500000 cP
@Shear Rate 1 1/s,
Temperature 482 °F
 1.15e+6 cP
@Shear Rate 1 1/s,
Temperature 230 °C
1.15e+6 cP
@Shear Rate 1 1/s,
Temperature 446 °F
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 57.0 MPa8270 psiISO 527-1/-2
Elongation at Break 2.4 %2.4 %ISO 527-1/-2
Tensile Modulus 4.70 GPa682 ksiISO 527-1/-2
Charpy Impact Unnotched 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 195 °C383 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Chang Chun Plastic PBT1200M General Purpose PBT
Chang Chun Plastic PBT1100L General Purpose PBT
Envalior Arnite® BM4 240 (PBT+PET)-MD20

PDSM9782 / 161403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.