MVR (330°C/2.16kg) 8 cm³/10 min; high viscosity; easy release; 'softening temperature (VST/B120)=203 °C; injection molding - melt temperature 330 - 340°C; Covers for brake lights and indicator lights; Recessed light fixtures/reflectors; Blade-type fuses; Headlamp reflectors/bezelsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |