MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 50H1 Natural L PA 66/6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: TECHNYL® B 50H1 Natural L is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is available in natural and other colors upon request.

Key Properties: UL94 V0 at 0.4mm; High ductility at low temperature; Excellent filling qualities

Benefits: This phosphorus and halogen free flame retardant grade, UL94 V0 at 0.4mm, offers excellent filling qualities together with good stiffness.

Applications: Connectivity : junction blocks, terminal blocks, connectors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Time 86400 sec
1.1 %
@Time 24.0 hour
ISO 62
Viscosity  20 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
20 cP
@Shear Rate 10000 1/s,
Temperature 536 °F
 20.1 cP
@Shear Rate 10000 1/s,
Temperature 270 °C
20.1 cP
@Shear Rate 10000 1/s,
Temperature 518 °F
 20.2 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
20.2 cP
@Shear Rate 10000 1/s,
Temperature 500 °F
 220 cP
@Shear Rate 100 1/s,
Temperature 280 °C
220 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 223 cP
@Shear Rate 100 1/s,
Temperature 270 °C
223 cP
@Shear Rate 100 1/s,
Temperature 518 °F
 224 cP
@Shear Rate 100 1/s,
Temperature 260 °C
224 cP
@Shear Rate 100 1/s,
Temperature 500 °F
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inIsotropy
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527 Type 1A
Tensile Strength, Yield 80.0 MPa11600 psiISO 527 Type 1A
 85.0 MPa12300 psiASTM D638
Tensile Stress at Strain  30.0 MPa
@Strain 1.5 %
4350 psi
@Strain 1.5 %
 65.0 MPa
@Strain 2.5 %
9430 psi
@Strain 2.5 %
 75.0 MPa
@Strain 3 %
10900 psi
@Strain 3 %
 78.0 MPa
@Strain 4 %
11300 psi
@Strain 4 %
Elongation at Break 10 %10 %ISO 527 Type 1A
 10 %10 %ASTM D638
Elongation at Yield 4.0 %4.0 %ISO 527 Type 1A
Tensile Modulus 3.60 GPa522 ksiISO 527 Type 1A
Flexural Strength 105 MPa15200 psiISO 178
 120 MPa17400 psiASTM D790
Flexural Modulus 3.65 GPa529 ksiISO 178
Izod Impact, Unnotched 0.0612 J/cm0.115 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.63.6IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 575 V575 VSol B; IEC 60112
 600 V600 VSol A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 242 °C468 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
ISO 1210
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
ISO 1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
ISO 1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
ISO 1210
Oxygen Index 33 %33 %ISO 4589
Glow Wire Test  650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
Ignition Temp; ISO 60695-2-13
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
Flammability Index; ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
Flammability Index; ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
Flammability Index; ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 245 - 255 °C473 - 491 °FCompression zone
 250 - 260 °C482 - 500 °FMixing zone
Feed Temperature 240 - 250 °C464 - 482 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® B 50H1 Natural L PA 66/6, Conditioned
Domo TECHNYL® B 50 H1 PA66/6, DRY
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH50
Nilit Polynil® C50 PA66/6 Co-Polymer
Nilit Polynil® C50L Externally Lubricated PA66/6

PSOLVAY853 / 218581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.