MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218 V30 Black 21 NS is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Mechanical performance; Heat stabilized

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0062 cm/cm0.0062 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527 Type 1A
Elongation at Break 6.0 %6.0 %ISO 527 Type 1A
Tensile Modulus 7.50 GPa1090 ksiISO 527 Type 1A
Flexural Strength 185 MPa26800 psiISO 178
Flexural Modulus 6.40 GPa928 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²30.9 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 8.80 J/cm²41.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inIEC 60243
Dissipation Factor 0.110.11IEC 60250
Comparative Tracking Index 600 V600 VSol A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Dry
Domo TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY

PSOLVAY831 / 218559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.