MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® C 216 V30 Black Z/4 is a polyamide 6, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.

Key Properties: Mechanical performance

Benefits: The product offers a good combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183/A
Water Absorption 1.05 %
@Time 86400 sec
1.05 %
@Time 24.0 hour
ISO 62
Viscosity  30 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 464 °F
 30 cP
@Shear Rate 10000 1/s,
Temperature 250 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 482 °F
 30 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 500 °F
 300 cP
@Shear Rate 100 1/s,
Temperature 240 °C
300 cP
@Shear Rate 100 1/s,
Temperature 464 °F
 400 cP
@Shear Rate 100 1/s,
Temperature 250 °C
400 cP
@Shear Rate 100 1/s,
Temperature 482 °F
 500 cP
@Shear Rate 100 1/s,
Temperature 260 °C
500 cP
@Shear Rate 100 1/s,
Temperature 500 °F
Linear Mold Shrinkage, Flow 0.0065 cm/cm0.0065 in/in
Linear Mold Shrinkage, Transverse 0.0035 cm/cm0.0035 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527 Type 1A
Tensile Stress at Strain  90.0 MPa
@Strain 1 %
13100 psi
@Strain 1 %
 150 MPa
@Strain 2 %
21800 psi
@Strain 2 %
 185 MPa
@Strain 3 %
26800 psi
@Strain 3 %
Elongation at Break 3.8 %3.8 %ISO 527 Type 1A
Tensile Modulus 9.60 GPa1390 ksiISO 527 Type 1A
Flexural Strength 235 MPa34100 psiISO 178
Flexural Modulus 8.00 GPa1160 ksiISO 178
 9.50 GPa1380 ksiASTM D790
Izod Impact, Unnotched 0.122 J/cm0.229 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.83.8IEC 60250
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 475 V475 VSol B; IEC 60112
 600 V600 VSol A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C432 °FISO 11357
Crystallization Temperature 190 °C374 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75/Af
 210 °C410 °FASTM D648
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
ISO 1210
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
ISO 1210
Oxygen Index 23 %23 %ISO 4589
Glow Wire Test 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
Flammability Index; ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 - 245 °C455 - 473 °FCompression zone
 245 - 250 °C473 - 482 °FMixing zone
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Conditioned

PSOLVAY857 / 218585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.