MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® C 216 V30 Black Z/4 is a polyamide 6, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.

Key Properties: Mechanical performance

Benefits: The product offers a good combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183/A
Water Absorption 1.05 %
@Time 86400 sec
ISO 62
Viscosity 30 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
 30 cP
@Shear Rate 10000 1/s,
Temperature 250 °C
 30 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
 300 cP
@Shear Rate 100 1/s,
Temperature 240 °C
 400 cP
@Shear Rate 100 1/s,
Temperature 250 °C
 500 cP
@Shear Rate 100 1/s,
Temperature 260 °C
Linear Mold Shrinkage, Flow 0.0065 cm/cm
Linear Mold Shrinkage, Transverse 0.0035 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527 Type 1A
Tensile Stress at Strain 90.0 MPa
@Strain 1 %
 150 MPa
@Strain 2 %
 185 MPa
@Strain 3 %
Elongation at Break 3.8 %ISO 527 Type 1A
Tensile Modulus 9600 MPaISO 527 Type 1A
Flexural Strength 235 MPaISO 178
Flexural Modulus 8000 MPaISO 178
 9500 MPaASTM D790
Izod Impact, Unnotched 12.2 J/mASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²ISO 180/1A
Charpy Impact Unnotched 100 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8IEC 60250
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 475 VSol B; IEC 60112
 600 VSol A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 222 °CISO 11357
Crystallization Temperature 190 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75/Af
 210 °CASTM D648
Flammability, UL94 HB
@Thickness 0.800 mm
ISO 1210
 HB
@Thickness 3.20 mm
ISO 1210
Oxygen Index 23 %ISO 4589
Glow Wire Test 650 °C
@Thickness 1.60 mm
Flammability Index; ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 - 245 °CCompression zone
 245 - 250 °CMixing zone
Feed Temperature 230 - 235 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Conditioned

PSOLVAY857 / 218585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.