MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 70G50HSLA BK039B PA66-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: 50% Glass Reinforced, Heat Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³DAM; ISO 1183
Melt Density 1.40 g/cc
@Temperature 295 °C
0.0506 lb/in³
@Temperature 563 °F
Water Absorption 4.2 %
@Thickness 2.00 mm
4.2 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
 0.80 %
@Thickness 2.00 mm,
Time 86400 sec
0.80 %
@Thickness 0.0787 in,
Time 24.0 hour
Immersion; DAM; Sim. to ISO 62
Moisture Absorption 1.20 %
@Thickness 2.00 mm
1.20 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 105 cm³/g1.05 dl/g96% sulfuric acid; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 300 MPa43500 psiH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 170 MPa24700 psi50% RH; ISO 527-1/-2
 240 MPa34800 psiDAM; ISO 527-1/-2
Elongation at Break 2.4 %2.4 %DAM; ISO 527-1/-2
 3.5 %3.5 %50% RH; ISO 527-1/-2
Tensile Modulus 13.0 GPa1890 ksi50% RH; ISO 527-1/-2
 17.0 GPa2470 ksiDAM; ISO 527-1/-2
Flexural Strength 280 MPa40600 psi50% RH; ISO 178
 400 MPa58000 psiDAM; ISO 178
 270 MPa
@Strain 3.5 %
39200 psi
@Strain 3.5 %
50% RH; ISO 178
Flexural Modulus 12.0 GPa1740 ksi50% RH; ISO 178
 16.0 GPa2320 ksiDAM; ISO 178
Compressive Strength 215 MPa31200 psiDAM; ISO 604
Poissons Ratio 0.330.3350% RH
 0.330.33DAM
Shear Strength 90.0 MPa13100 psiDAM; ASTM D 732
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Puncture Energy 10.0 J
@Temperature 23.0 °C
7.38 ft-lb
@Temperature 73.4 °F
DAM; ISO 6603-2
Tensile Creep Modulus, 1 hour 10000 MPa1.45e+6 psi1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 8000 MPa1.16e+6 psi1000h; 50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 4.00e+14 ohm4.00e+14 ohm50% RH; IEC 62631-3-2
Dielectric Strength 30.0 kV/mm762 kV/inDAM; IEC 60243-1
Comparative Tracking Index 500 V500 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 9.00 µm/m-°C5.00 µin/in-°FDAM; ISO 11359-1/-2
 13.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
7.22 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 19.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
10.6 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ASTM E 831
 19.0 µm/m-°C
@Temperature 55.0 - 160 °C
10.6 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C40.0 µin/in-°FDAM; ISO 11359-1/-2
 42.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
23.3 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 61.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.9 µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ASTM E 831
 114 µm/m-°C
@Temperature 55.0 - 160 °C
63.3 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Specific Heat Capacity 1.87 J/g-°C
@Temperature 295 °C
0.447 BTU/lb-°F
@Temperature 563 °F
Melt
Thermal Conductivity 0.460 W/m-K3.19 BTU-in/hr-ft²-°FSolid
 0.310 W/m-K
@Temperature 295 °C
2.15 BTU-in/hr-ft²-°F
@Temperature 563 °F
Melt
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °C502 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FDAM; ISO 75-1/-2
Vicat Softening Point 255 °C491 °F50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 20.0 °C68.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 65.0 °C149 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.830 mm
HB
@Thickness 0.0327 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Oxygen Index 24 %24 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 295 °C563 °FOptimum, Injection
 285 - 305 °C545 - 581 °FRange, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)6.5VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
Fogging (mg)0.4G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66,GF50,M1CGHR,S10-160
Max. screw tangential speed (m/s)0.2Injection
Odor Class3VDA 270
Part Marking Code>PA66-GF50<ISO 11469
PolymerPA66-GF50
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66-GF50ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® FG70G50HSLA BK309 PA66-GF50
Celanese Zytel® 70G35HSLRA4 BK267 PA66-GF35
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced Nylon 6
Celanese Zytel® 73G50HSLA BK416 PA6-GF50
Celanese Zytel® 101 NC010 PA66

PDSX5343 / 197983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.