MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: ISO data as provided by the manufacturer, Eastman Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
Linear Mold Shrinkage, Transverse 0.0075 cm/cm0.0075 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi50 mm/min
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 4.8 %4.8 %
Tensile Modulus 1.54 GPa223 ksi1mm/min
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched 5.50 J/cm²26.2 ft-lb/in²Partial Break
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
Partial Break
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 87.0 µm/m-°C
@Temperature 20.0 °C
48.3 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 83.0 µm/m-°C
@Temperature 20.0 °C
46.1 µin/in-°F
@Temperature 68.0 °F
Melting Point 241 °C466 °F
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °F
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °F
Vicat Softening Point 106 °C223 °F
Glass Transition Temp, Tg 111 °C232 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate
Toyobo A1061D Thermoplastic Polyurethane Elastomer, Injection Grade
A. Schulman Diamond DIAMALOY 223U UV Stabilized, PC/PET Alloy

PEAT6053 / 21292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.