MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo A1061D Thermoplastic Polyurethane Elastomer, Injection Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.

Information provided by Toyobo Co., Ltd

Key Words: TPUR; Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength, Ultimate 46.0 MPa6670 psiASTM D638
Tensile Stress at Strain 20.6 MPa
@Strain 100 %
2990 psi
@Strain 100 %
ASTM D638
Elongation at Break 450 %450 %ASTM D638
Tear Strength 216 kN/m1230 pliASTM D624
Taber Abrasion, mg/1000 Cycles 7070H22
Compression Set 40 %40 %ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 135 °C275 °FASTM D1525
Brittleness Temperature <= -65.0 °C<= -85.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
A. Schulman Alcryn® 2160 BK Melt Processable Rubber
Toyobo A3080A Thermoplastic Polyurethane Elastomer, Injection Grade
Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade
Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade

PTOY08 / 70680

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.