MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® NEXAR™ MD9150 Polymer Barrier Membrane  (discontinued **)
Categories: Polymer

Material Notes: NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and dehumidification applications such as water management and breathable fabrics. They have a high resistance to chlorine, making water treatment a target market.

This data sheet is for membranes, but MD9150 is also available in solution for coating or laminating purposes.

Information provided by Kraton®.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 3.10 MPa450 psiWet
 10.0 MPa1450 psiDry
Tensile Strength, Yield 13.0 MPa1890 psiDry
Elongation at Break 70 %70 %Wet
 100 %100 %Dry
Elongation at Yield 4 %4 %Dry
Modulus of Elasticity 0.0750 GPa10.9 ksiWet
 0.480 GPa69.6 ksiDry
 
Descriptive Properties
Ion Exchange Capacity1.5 meq/g

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ HP 3704 High Performance Thermoplastic Elastomer
Kraton® NEXAR™ MD9200 Polymer Barrier Membrane
Mitsui HILET™ 2221 Porous Polyethylene Membrane
Mitsui HILET™ 1351D Porous Polyethylene Membrane
AlphaGary Evoprene™ HP 3702 High Performance Thermoplastic Elastomer

PKRA9930 / 133508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.