MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis EDISTIR PD RK4122H High Impact Polystyrene (HIPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Symbol according to ISO 1043-1: S/B
Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23

UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stability in the injection molding process and good mechanical properties.

Applications: Examples of applications are TV back covers, printers and copiers.

Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min
Elongation at Break 30 %30 %Nominal
Tensile Modulus 2.45 GPa355 ksi1 mm/min
Charpy Impact Unnotched 8.50 J/cm²40.5 ft-lb/in²
 7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant 2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm1650 kV/in
Dissipation Factor 0.00060
@Frequency 100 Hz
0.00060
@Frequency 100 Hz
Comparative Tracking Index 475 V475 V
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °F50°C/hr; 50N
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americas Styrenics Styron® 425 High Impact Polystyrene
Videolar-Innova 825 E High Impact Polystyrene (HIPS)
Videolar-Innova 825 High Impact Polystyrene (HIPS)
Aclo Accucomp Polystyrene HS0600L High Impact
Americas Styrenics EA6740 High Impact Polystyrene

PENI59 / 35866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.