MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Filler Content 8.0 %8.0 %Carbon Fiber Reinforcement
Water Absorption 0.25 %
@Thickness 3.18 mm
0.25 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.9 MPa9990 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 4.83 GPa701 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 4.69 GPa680 ksiASTM D790
Izod Impact, Notched 0.640 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 - 1.00e+6 ohm-cm10000 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
@Thickness 6.35 mm
210 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
@Thickness 6.35 mm
205 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 232 °C430 - 450 °F
 
Descriptive Properties
FeaturesAntistatic
 ESD Protection
FormsPellets
Generic MaterialABS
Generic NameAcrylonitrile Butadiene Styrene (ABS)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Automotive Under the Hood
 Business Equipment
 Electrical/Electronic Applications
 Housings
 Printer Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS)
Avient Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS)
Aclo Accutech ABS ABS831G10L Glass Reinforced
Avient Maxxam™ PPC-10G Black Polypropylene Copolymer (PP Copolymer)
Aclo Accutech ABS ABS831G20L Glass Reinforced

PH0POL0706 / 145275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.