MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Devcon Zip Patch™ Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emergency Repair Products

Comments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-use, fast setting patch kit. Make permanent, waterproof field repairs to pipes, tanks and containers, Excellent adhesion to iron, steel, stainless steel, titanium, fiberglass, aluminum, wood, ceramics, composites, acrylics, PVC and most other plastics. Minimal surface preparation.

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Viscosity 17000 cP17000 cPwith hardener
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength, Ultimate 69.6 MPa10100 psiASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Yield Strength 131 MPa19000 psiASTM D790
Adhesive Bond Strength 31.7 MPa4600 psiAdhesive tensile shear strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 43.543.5ASTM D150
Dielectric Strength 9.84 kV/mm250 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 115 µm/m-°C
@Temperature 20.0 °C
63.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.715 W/m-K4.96 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 93.3 °C200 °FOperating Temperature
Shrinkage 0.10 %0.10 %During Cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 °C70.0 °F
Pot Life 5.00 min
@Temperature 23.9 °C
5.00 min
@Temperature 75.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Devcon Underwater Repair Putty (UW) Epoxy
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Abatron AboCast/AboCure 8502-1 Epoxy
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy

PITWX16 / 48503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.