MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis ME1244 Medium Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications: ME1244 is intended for: foam or foam-skin insulation for telephone singles with typical expansion of 35-40%, and dry core and petroleum jelly filled cables. ME1244 meets these requirements when processed using sound extrusion practice and testing procedure: ASTM D1248 Type II, Class A, Category 4, BS 6234: Type 03 EN 50290-2-23 IEC 60708 NF C32-060 ISO 1872-PE, KEHN, 33-D006.

Former trade name for this product was Borcell™.

Information provided by Borealis AG

Key Words: MDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.934 g/cc0.0337 lb/in³base resin; ISO 1872-2/ISO 1183
 0.937 g/cc0.0339 lb/in³compound; ISO 1872-2/ISO 1183
Thermal Stress Crack Resistance 1.50 hour
@Temperature 105 °C
1.50 hour
@Temperature 221 °F
IEC 60811-4-2/A
Oxidative Induction Time (OIT) 50 min
@Temperature 200 °C
50 min
@Temperature 392 °F
IEC 60811-4-2/B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 11.0 MPa1600 psi50mm/min; ISO 527
 11.0 MPa1600 psi50mm/min, expanded 35% insulation; IEC 60811-1-1
Elongation at Break 500 %500 %50mm/min; ISO 527
 500 %500 %50mm/min, 35% expanded insulation; IEC 60811-1-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.31
@Frequency 1e+6 Hz
2.31
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
IEC 60250
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °Fconductor preheating temperature
Zone 1 155 °C311 °F
Zone 2 170 °C338 °F
Zone 3 185 °C365 °F
Zone 4 195 °C383 °F
Die Temperature 195 °C383 °F
Melt Temperature 195 - 200 °C383 - 392 °F
 
Descriptive Properties
Petroleum Jelly Absorption (%)10IEC 60811-4-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BorSafe™ ME3445 Medium Density Polyethylene
Borealis Borstar® FB1350 Medium Density Polyethylene
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
Overview of materials for Medium Density Polyethylene (MDPE), Molded
A. Schulman CP812 Linear, Medium-Density Polyethylene

PBOREA360 / 108620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.