MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: ABS for sheet and profile extrusion

High impact resistance, excellent heat resistance, excellent dimensional stability and processability

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D 955
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.0 MPa3340 psiASTM D 638
Tensile Strength, Yield 36.0 MPa5220 psiASTM D 638
Elongation at Break 20 %20 %ASTM D 638
Flexural Modulus 2.20 GPa319 ksiASTM D 790
Izod Impact, Notched  3.00 J/cm
@Temperature 0.000 °C
5.62 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 3.50 J/cm
@Temperature 23.0 °C
6.56 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  102 °C
@Load 5.00 kg
216 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 114 °C
@Load 0.999 kg
237 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Test 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zeus FEP Tubing and Drawn Fiber
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength
Baystar™ 7195 High Density Polyethylene, Specialty Extrusion Resin
BASF Ultramid® KR 4350 PA6/6T (Dry)

PCOSSA827 / 156417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.