MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alclad Aluminum 3003-H112
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Key Words: UNS A83003
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.73 g/cc0.0986 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  >= 100 MPa
@Thickness 50.8 - 76.2 mm
>= 14500 psi
@Thickness 2.00 - 3.00 in
 >= 105 MPa
@Thickness 12.7 - 50.8 mm
>= 15200 psi
@Thickness 0.500 - 2.00 in
 >= 110 MPa
@Thickness 6.35 - 12.7 mm
>= 16000 psi
@Thickness 0.250 - 0.499 in
Tensile Strength, Yield  >= 41.0 MPa
@Thickness 12.7 - 50.8 mm
>= 5950 psi
@Thickness 0.500 - 2.00 in
 >= 41.0 MPa
@Thickness 50.8 - 76.2 mm
>= 5950 psi
@Thickness 2.00 - 3.00 in
 >= 62.0 MPa
@Thickness 6.35 - 12.7 mm
>= 8990 psi
@Thickness 0.250 - 0.499 in
Elongation at Break  8.0 %
@Thickness 6.35 - 12.7 mm
8.0 %
@Thickness 0.250 - 0.499 in
 12 %
@Thickness 12.7 - 50.8 mm
12 %
@Thickness 0.500 - 2.00 in
 18 %
@Thickness 50.8 - 76.2 mm
18 %
@Thickness 2.00 - 3.00 in
Modulus of Elasticity 70.0 GPa10200 ksi
Poissons Ratio <= 0.33<= 0.33
Shear Modulus 25.0 GPa3630 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.5 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.9 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.2 µm/m-°C
@Temperature 20.0 - 100 °C
12.9 µin/in-°F
@Temperature 68.0 - 212 °F
 24.1 µm/m-°C
@Temperature 20.0 - 200 °C
13.4 µin/in-°F
@Temperature 68.0 - 392 °F
 25.1 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.893 J/g-°C0.213 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 98.05 - 99.2 %98.05 - 99.2 %
Copper, Cu <= 0.10 %<= 0.10 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Si+Fe <= 0.70 %<= 0.70 %
Zinc, Zn 0.80 - 1.3 %0.80 - 1.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alclad Aluminum 3003-H12
Alclad Aluminum 3003-H14
Aluminum 3003-H112
Alclad Aluminum 3003-O
Alclad Aluminum 3003-H18

MA3003AH112 / 109178

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.