MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics. It is also available in heat stabilized (Ultramid 8331G HI HS) and/or pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Melt Density 1.16 g/cc
@Temperature >=220 °C
0.0419 lb/in³
@Temperature >=428 °F
ISO 1183
Water Absorption 0.90 %0.90 %24 hour; ISO Test
 5.5 %5.5 %ISO 62
Moisture Absorption at Equilibrium 1.5 %1.5 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM Test
Tensile Strength at Break 152 MPa22000 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 145 MPa21000 psi5mm/min; ISO 527
Elongation at Break 3.5 %3.5 %5mm/min; ISO 527
 3.5 %3.5 %0.2 in/min; ASTM Test
Tensile Modulus 9.30 GPa1350 ksi1mm/min; ISO 527
 2.66 GPa
@Temperature 120 °C
386 ksi
@Temperature 248 °F
ISO Data
 9.20 GPa
@Temperature -40.0 °C
1330 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 215 MPa31200 psiISO Data
 241 MPa35000 psiASTM Test
 89.0 MPa
@Temperature 120 °C
12900 psi
@Temperature 248 °F
ASTM Test
 105 MPa
@Temperature 93.0 °C
15200 psi
@Temperature 199 °F
ASTM Test
 130 MPa
@Temperature 65.0 °C
18900 psi
@Temperature 149 °F
ASTM Test
 310 MPa
@Temperature -40.0 °C
45000 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 7.20 GPa1040 ksiISO Data
 8.00 GPa1160 ksiASTM Test
 3.04 GPa
@Temperature 120 °C
441 ksi
@Temperature 248 °F
ASTM Test
 3.28 GPa
@Temperature 93.0 °C
476 ksi
@Temperature 199 °F
ASTM Test
 4.04 GPa
@Temperature 65.0 °C
586 ksi
@Temperature 149 °F
ASTM Test
Izod Impact, Notched 2.39 J/cm
@Thickness 3.17 mm
4.48 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 21.0 kJ/m²9.99 ft-lb/in²ISO Test
 14.0 kJ/m²
@Temperature -40.0 °C
6.66 ft-lb/in²
@Temperature -40.0 °F
ISO Test
Charpy Impact Unnotched 7.80 J/cm²37.1 ft-lb/in²ISO 179
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+9 Hz
3.8
@Frequency 1e+9 Hz
ASTM Data
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM Data
Dielectric Strength 43.0 kV/mm1090 kV/inIEC 60243-1
Dissipation Factor  0.010
@Frequency 1e+9 Hz
0.010
@Frequency 1e+9 Hz
ASTM Data
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM Data
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C13.3 µin/in-°FISO 11359
CTE, linear, Transverse to Flow 84.0 µm/m-°C46.7 µin/in-°FISO 11359
Specific Heat Capacity 1.958 J/g-°C0.4680 BTU/lb-°FMelt
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FMelt
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75
 210 °C410 °FASTM Test
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 95.0 °C203 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® 8351 HS BK 106 PA6 (Dry)
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)

PBASF9203 / 84967

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.