MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Edistir R 540E Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection moldings.

Designation: Thermoplastics ISO 2897-PS-I,G,093-03-07-18

Applications: To be used in industrial panels for appliances and buildings. Injection molding of shoe heels.

R 540E satisfies UL94 HB at 1.5 mm (internal test).

This grade in natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (included the EEC Directive 90/128 and following amendments).

Information provided by Polimeri Europa

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption <= 0.10 %<= 0.10 %24 hours - 23°C; ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inInternal Method
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7070ISO 2039/2
Tensile Strength at Break 29.0 MPa4210 psi50 mm/min; ISO 527
Tensile Strength, Yield 24.0 MPa3480 psi50 mm/min; ISO 527
Elongation at Break 60 %60 %50 mm/min; ISO 527
Tensile Modulus 2.00 GPa290 ksi1 mm/min; ISO 527
Flexural Strength 43.0 MPa6240 psi2 mm/min; ISO 178
Izod Impact, Notched 1.00 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.87 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
2.86 ft-lb/in²
@Thickness 0.157 in,
Temperature -22.0 °F
ISO 180/1A
 8.00 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
3.81 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+15 ohm-cm7.00e+15 ohm-cmIEC 60093
Surface Resistance 1.50e+15 ohm1.50e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 50 Hz
2.5
@Frequency 50 Hz
IEC 60250
Dielectric Strength 65.0 kV/mm1650 kV/inIEC 60243
Dissipation Factor 0.00030
@Frequency 50 Hz
0.00030
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D 696
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °F120°C/h; ASTM D 648
Vicat Softening Point 92.0 °C198 °F50 N - 50°C/h; ISO 306/B
 100 °C212 °F10 N - 50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL94
Glow Wire Test 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
IEC 60695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °FExtrusion
 210 - 260 °C410 - 500 °FInjection Molding
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °FInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Edistir R 850E Polystyrene
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
Versalis Edistir N 1910 Polystyrene
Versalis Edistir N 2982 Polystyrene
Resirene Resirene® 9720 High Impact Polystyrene

PENI409 / 35846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.