MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7050-T7651
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: 7050 has very high strength coupled with high resistance to exfoliation corrosion and stress-corrosion cracking, high fracture toughness, and fatigue resistance. This leads to applications in aircraft structures.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97050; ISO AlZn6CuMgZr; Aluminium 7050-T7651; AA7050-T7651; Al7050-T7651
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 147147500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 187187Converted from Brinell Hardness Value
Hardness, Rockwell A 5353Converted from Brinell Hardness Value
Hardness, Rockwell B 8686Converted from Brinell Hardness Value
Hardness, Vickers 171171Converted from Brinell Hardness Value
Tensile Strength, Ultimate 552 MPa80000 psiAA; Typical
Tensile Strength, Yield 490 MPa71000 psiAA; Typical
Elongation at Break 11 %
@Diameter 12.7 mm
11 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 71.7 GPa10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33
Fracture Toughness 20.9 MPa-m½19.0 ksi-in½average; S-L
 26.0 MPa-m½23.7 ksi-in½K(IC) in S-L Direction
 26.4 MPa-m½24.0 ksi-in½average; T-L
 30.8 MPa-m½28.0 ksi-in½average; L-T
 31.0 MPa-m½28.2 ksi-in½K(IC) in T-L Direction
 34.0 MPa-m½30.9 ksi-in½K(IC) in L-T Direction
Shear Modulus 26.9 GPa3900 ksi
Shear Strength 324 MPa47000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 ohm-cm0.00000440 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.1 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.0 µm/m-°C
@Temperature 20.0 - 100 °C
12.8 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.6 µin/in-°F
@Temperature 68.0 - 392 °F
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
14.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.860 J/g-°C0.206 BTU/lb-°F
Thermal Conductivity 153 W/m-K1060 BTU-in/hr-ft²-°F
Melting Point 488 - 629.4 °C910 - 1165 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 488 °C910 °FAA; Typical
Liquidus 629.4 °C1165 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 477 °C890 °F
Aging Temperature 121 - 177 °C250 - 350 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 87.3 - 90.3 %87.3 - 90.3 %As remainder
Chromium, Cr <= 0.04 %<= 0.04 %
Copper, Cu 2.0 - 2.6 %2.0 - 2.6 %
Iron, Fe <= 0.15 %<= 0.15 %
Magnesium, Mg 1.9 - 2.6 %1.9 - 2.6 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.12 %<= 0.12 %
Titanium, Ti <= 0.06 %<= 0.06 %
Zinc, Zn 5.7 - 6.7 %5.7 - 6.7 %
Zirconium, Zr 0.08 - 0.15 %0.08 - 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 7050-T7451 (7050-T73651)
Aluminum 6061-T6; 6061-T651
Aluminum 7050-T74
Aluminum 7050-T73651 plate

MA7050T765 / 9578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.