MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron ROCKWELD 55-27 A/B Structural Adhesive Putty; Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: ROCKWELD 55-27 is a 2-component epoxy system with low density, high-strength, and no shrinkage. It is a structural adhesive putty for sculpturing, repairs and restoration of stone, concrete and masonry, terracotta, and ceramics. This clay-like putty can be used to build up, model, patch, or replace shapes or parts of any structural or decorative element. Statues, architectural decorations, ornaments and mosaics can be repaired and restored using ROCKWELD. Broken stairs, railings, cracked and splitting concrete patios, floors, and walls are only a few examples of ROCKWELD applications. Tenacious adhesion to metal and wood also allows the repair of items made of different materials. The clay-like putty hardens without shrinking. It can be built up several inches thick. Thicker layers can generate too much heat that may impair final properties of the material. The new material adheres permanently to the old one. ROCKWELD can be shaped by hand because of its modeling clay consistency. It does not slump or sag when being applied to vertical surfaces. After hardening this material can be sanded by hand using coarse sandpaper (100 grit or less) or any mechanical tools such as circular or belt sanders. Tools like knives or files are not recommended because of the high abrasiveness of ROCKWELD. ROCKWELD can be primed and coated using any solvent or waterborne paint. Slight sanding is recommended, in some cases, as a surface preparation. To match the color of the object to be repaired, any dry pigment or pigment dispersion compatible with epoxy systems can be admixed to ROCKWELD. It can be blended with pebble stone, gravel, or concrete particles. It can be reinforced with inserts, rods, wires, and other reinforcing elements. ROCKWELD is chemically resistant and unaffected by atmospheric conditions and soft and salt water. ROCKWELD bonds to wet as well as dry surfaces.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Volatiles 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength at Break 15.9 MPa2300 psi
Elongation at Break 2.8 %2.8 %
Modulus of Elasticity 0.565 GPa82.0 ksi
Flexural Strength 27.6 MPa4000 psi
Compressive Strength 50.3 MPa7300 psi
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 93.0 - 105 °C
1.00 - 2.00 hour
@Temperature 199 - 221 °F
 10080 min
@Temperature 20.0 °C
168.0 hour
@Temperature 68.0 °F
(7 Days)
Pot Life 50 min
@Temperature 25.0 °C
50 min
@Temperature 77.0 °F
100 g
 
Descriptive Properties
ColorGray
Hardening Time (min)120-240at room temperature
Induction Period (min)>= 5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A500 Steel, grade A, Round Structural Tubing
Abatron AboCast 50-11/AboCure 50-4 Epoxy
Abatron AboCast 10-5/AboCure 3-4 Epoxy
ASTM A500 Steel, grade A, shaped structural tubing
ASTM A500 Steel, grade B, shaped structural tubing

PABC911 / 107895

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.