MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® NRG 6001 PA 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: VESTAMID®NRG 6001 is a plasticized PA 12 compound with heat and light stabilizers for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications (e.g. for Umbilicals ). VESTAMID®NRG 6001 is characterized by easy processing and good dimensional control during pipe extrusion, especially when processing of multi layer tubes. This PA12 compound is optimized for excellent bonding to NeoflonTM EFEP RP-5000 (a registered trademark of Daikin Industries ) Properties of compounds based on polyamide 12 vary little with changing humidity due to low moisture absorption Parts made of the described semi-crystalline material are characterized by exceptional impact strength, low coefficient of sliding friction and good chemical resistance. VESTAMID®NRG 6001 is supplied ready for use in moisture-proof bags. The recommended process temperature for extrusion is 220°C to 260°C.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psiISO 527
Elongation at Break >= 150 %>= 150 %ISO 527
Tensile Modulus 0.390 GPa56.6 ksiISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.540 J/cm²
@Temperature -40.0 °C
2.57 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.720 J/cm²
@Temperature -30.0 °C
3.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 9.40 J/cm²
@Temperature 0.000 °C
44.7 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 12.5 J/cm²
@Temperature 23.0 °C
59.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 172 °C342 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FISO 75
Vicat Softening Point  124 °C
@Load 5.10 kg
255 °F
@Load 11.2 lb
Method B; ISO 306
 164 °C
@Load 1.02 kg
327 °F
@Load 2.25 lb
Method A; ISO 306
 
Descriptive Properties
ColorNatural color

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® NRG 1001 PA 12
Evonik VESTAMID® NRG 3001 PA 12
Evonik VESTAMID® EX9200 PA 12
Evonik VESTAMID® LX9008 PA 12
GEHR Plastics PA 12 TR Transparent Nylon 12

PEVONIL274 / 196478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.