MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100)
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese and nitrogen additions are partial substitutes for nickel making them more economical alloys. Because they possess a very desirable combination of economy plus good mechanical properties and corrosion resistance properties, they have been used in a wide variety of consumer and transportation applications.

This austenitic structure achieves significant strengthening through cold working of the material to produce the transformation to a stronger martensitic structure. Type 201 is resistant to a wide variety of mild to moderately corrosive media.

Typical applications for Types 201 and 201L are cookware bodies/lids, hose clamps, piston rings, transit car structural member, transit car roofing/siding, thermal window spacers, air bag containers, and truck trailer posts and door frames.

Information provided by Allegheny Ludlum Corporation.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C  34.5
@Temperature 23.0 °C
34.5
@Temperature 73.4 °F
 34.5
@Temperature 23.0 °C
34.5
@Temperature 73.4 °F
Tensile Strength, Ultimate  1044 MPa
@Temperature 23.0 °C
151400 psi
@Temperature 73.4 °F
 1045 MPa
@Temperature 23.0 °C
151600 psi
@Temperature 73.4 °F
Tensile Strength, Yield  795 MPa
@Temperature 23.0 °C
115000 psi
@Temperature 73.4 °F
 837 MPa
@Temperature 23.0 °C
121000 psi
@Temperature 73.4 °F
Elongation at Break  17.5 %
@Temperature 23.0 °C
17.5 %
@Temperature 73.4 °F
 22.3 %
@Temperature 23.0 °C
22.3 %
@Temperature 73.4 °F
Modulus of Elasticity 192 GPa27800 ksi
Compressive Yield Strength 503 MPa73000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000670 ohm-cm0.0000670 ohm-cm
Magnetic Permeability 1.961.96D.C. Permeability (m at 200 H)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.22 µin/in-°F
@Temperature 68.0 - 212 °F
 18.0 µm/m-°C
@Temperature 20.0 - 316 °C
10.0 µin/in-°F
@Temperature 68.0 - 601 °F
 18.0 µm/m-°C
@Temperature 20.0 - 358 °C
10.0 µin/in-°F
@Temperature 68.0 - 676 °F
 20.3 µm/m-°C
@Temperature 20.0 - 871 °C
11.3 µin/in-°F
@Temperature 68.0 - 1600 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 23.0 W/m-K
@Temperature 500 °C
160 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 72 %72 %as balance
Manganese, Mn 5.5 - 7.5 %5.5 - 7.5 %
Nickel, Ni 3.5 - 5.5 %3.5 - 5.5 %
Nitrogen, N <= 0.25 %<= 0.25 %
Silicon, Si <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103)
AK Steel 201 Austenitic Stainless steel
AK Steel 201LN Austenitic Stainless steel
AK Steel 301 Austenitic Stainless steel

NL2013 / 17811

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.