MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping capacity.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
Melt Flow 25 g/10 min
@Load 8.70 kg,
Temperature 190 °C
25 g/10 min
@Load 19.2 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585
Tensile Strength at Break 24.4 MPa3540 psi
Elongation at Break 610 %610 %
50% Modulus 5.50 MPa
@Strain 50 %
5.50 MPa
@Strain 50 %
100% Modulus 5.90 MPa
@Strain 100 %
856 psi
@Strain 100 %
300% Modulus 9.70 MPa
@Strain 300 %
1410 psi
@Strain 300 %
Tear Strength 127 kN/m725 pli
Taber Abrasion, mg/1000 Cycles 5050H22 Wheel
Compression Set  30 %
@Temperature 23.0 °C
30 %
@Temperature 73.4 °F
 80 %
@Temperature 70.0 °C
80 %
@Temperature 158 °F
Tensile Set 80 %80 %Elongation set after break
 
Thermal PropertiesMetricEnglishComments
CTE, linear 159 µm/m-°C
@Temperature 20.0 °C
88.3 µin/in-°F
@Temperature 68.0 °F
Vicat Softening Point 67.0 °C153 °F
Glass Transition Temp, Tg -24.0 °C-11.2 °F
Clash Berg Stiffness Temperature -38.0 °C-36.4 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based
Covestro Platilon® 4201 AU Polyurethane (Ether) Film
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact

PDW276 / 34444

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.