MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: PELLETHANE® 2354-65D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane and acrylic enamels or water based elastomeric paints without a primer.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 224 °C
24 g/10 min
@Load 11.0 lb,
Temperature 435 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength at Break 40.0 MPa5800 psi
Elongation at Break 430 %430 %
50% Modulus 16.5 MPa
@Strain 50 %
16.5 MPa
@Strain 50 %
100% Modulus 19.3 MPa
@Strain 100 %
2800 psi
@Strain 100 %
300% Modulus 25.9 MPa
@Strain 300 %
3760 psi
@Strain 300 %
Tear Strength 210 kN/m1200 pli
Taber Abrasion, mg/1000 Cycles 4040H22 Wheel
Compression Set  25 %
@Temperature 70.0 °C
25 %
@Temperature 158 °F
 25 %
@Temperature 23.0 °C
25 %
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C
@Temperature 20.0 °C
65.0 µin/in-°F
@Temperature 68.0 °F
Vicat Softening Point 141 °C286 °F
Clash Berg Stiffness Temperature -17.8 °C-0.0400 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)

PDW279 / 34447

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.