MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, Automotive

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Melt Index of Compound 22 g/10 min
@Load 1.20 kg,
Temperature 224 °C
22 g/10 min
@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63 - 7363 - 73ASTM D2240
Tensile Strength, Ultimate 37.9 MPa5500 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
50% Modulus 21.4 MPa
@Strain 50 %
21.4 MPa
@Strain 50 %
ASTM D412
100% Modulus 22.8 MPa
@Strain 100 %
3310 psi
@Strain 100 %
ASTM D412
300% Modulus 30.3 MPa
@Strain 300 %
4390 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.207 GPa30.0 ksiASTM D790
Tear Strength 201 kN/m1150 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 5656H-22 wheel (coarser); ASTM D1044
Compression Set 82 %
@Temperature 70.0 °C
82 %
@Temperature 158 °F
22 hrs.; ASTM D395, Method B
 46 %
@Temperature 25.0 °C,
Time 79200 sec
46 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395, Method B
Tensile Set 130 %130 %Elongation Set After Break; ASTM D412
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 µm/m-°C
@Temperature 20.0 °C
66.1 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Vicat Softening Point 143 °C289 °FASTM D1525
Glass Transition Temp, Tg -28.0 °C-18.4 °FDSC
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 227 °C410 - 441 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer

PDW299 / 34467

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.