MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Flexible 86509  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Flexible Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474ASTM D2240
 66
@Time 15.0 sec
66
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psi510 mm/min; ASTM D638
Elongation at Break 350 %350 %510 mm/min; ASTM D638
Tear Strength 40.3 kN/m230 pliDie C, 510 mm/min; ASTM D624
 
Processing PropertiesMetricEnglishComments
Melt Temperature 174 - 179 °C345 - 354 °F
 
Descriptive Properties
FeaturesLow to No Migration
 Low to No Odor
FormsPellets
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliance Components
 Appliances
 Gaskets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Flexible Grade
Geon® Performance Solutions Vinyl Flexible XV3830 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible R7426A Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible D6500 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible

PH1PN8299 / 102135

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.