MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 60% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 - 1.85 g/cc0.0448 - 0.0668 lb/in³Average value: 1.70 g/cc Grade Count:116
Filler Content 60.0 %60.0 %Average value: 60.0 % Grade Count:22
Water Absorption 0.350 - 3.70 %0.350 - 3.70 %Average value: 1.09 % Grade Count:61
Moisture Absorption at Equilibrium 0.700 - 1.20 %0.700 - 1.20 %Average value: 1.04 % Grade Count:15
 0.800 - 1.20 %
@Temperature 70.0 - 70.0 °C
0.800 - 1.20 %
@Temperature 158 - 158 °F
Average value: 0.980 % Grade Count:10
Water Absorption at Saturation 2.90 - 4.00 %2.90 - 4.00 %Average value: 3.41 % Grade Count:46
Maximum Moisture Content 0.150 - 0.2000.150 - 0.200Average value: 0.163 Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.0200 cm/cm0.000500 - 0.0200 in/inAverage value: 0.00261 cm/cm Grade Count:74
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm0.00100 - 0.00900 in/inAverage value: 0.00385 cm/cm Grade Count:44
Spiral Flow 47.0 - 468 cm18.5 - 184 inAverage value: 121 cm Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120 - 122120 - 122Average value: 121 Grade Count:18
Ball Indentation Hardness 260 - 420 MPa37700 - 60900 psiAverage value: 327 MPa Grade Count:41
Tensile Strength, Ultimate 130 - 813 MPa18900 - 118000 psiAverage value: 258 MPa Grade Count:93
 75.0 - 353.701 MPa
@Temperature -40.0 - 150 °C
10900 - 51300.1 psi
@Temperature -40.0 - 302 °F
Average value: 153 MPa Grade Count:4
Tensile Strength, Yield 159 - 285 MPa23000 - 41300 psiAverage value: 232 MPa Grade Count:24
 144.79 - 144.79 MPa
@Temperature 93.3 - 93.3 °C
21000 - 21000 psi
@Temperature 200 - 200 °F
Average value: 145 MPa Grade Count:1
Elongation at Break 1.00 - 4.00 %1.00 - 4.00 %Average value: 1.96 % Grade Count:108
 1.80 - 7.50 %
@Temperature 4.44 - 150 °C
1.80 - 7.50 %
@Temperature 40.0 - 302 °F
Average value: 3.89 % Grade Count:4
Modulus of Elasticity 10.2 - 33.4 GPa1480 - 4840 ksiAverage value: 21.1 GPa Grade Count:88
 5.80 - 20.8566 GPa
@Temperature -40.0 - 150 °C
841 - 3025.05 ksi
@Temperature -40.0 - 302 °F
Average value: 12.1 GPa Grade Count:5
Flexural Yield Strength 241 - 793 MPa35000 - 115000 psiAverage value: 375 MPa Grade Count:65
 227.527 - 544.686 MPa
@Temperature -40.0 - 121 °C
33000.1 - 79000.1 psi
@Temperature -40.0 - 250 °F
Average value: 344 MPa Grade Count:2
Flexural Modulus 9.30 - 32.0 GPa1350 - 4640 ksiAverage value: 18.4 GPa Grade Count:66
 10.2732 - 19.3053 GPa
@Temperature -40.0 - 121 °C
1490.02 - 2800.04 ksi
@Temperature -40.0 - 250 °F
Average value: 14.4 GPa Grade Count:3
Izod Impact, Notched 1.13 - 7.00 J/cm2.11 - 13.1 ft-lb/inAverage value: 2.72 J/cm Grade Count:39
 7.21 - 7.68816 J/cm
@Temperature -51.1 - 149 °C
13.5 - 14.4031 ft-lb/in
@Temperature -60.0 - 300 °F
Average value: 7.51 J/cm Grade Count:2
Izod Impact, Unnotched 10.7 - 5340 J/cm20.0 - 10000 ft-lb/inAverage value: 20.0 J/cm Grade Count:24
Izod Impact, Notched (ISO) 11.0 - 30.0 kJ/m²5.23 - 14.3 ft-lb/in²Average value: 15.1 kJ/m² Grade Count:5
Charpy Impact Unnotched 5.50 - 15.0 J/cm²26.2 - 71.4 ft-lb/in²Average value: 8.64 J/cm² Grade Count:68
 6.00 - 10.92 J/cm²
@Temperature -30.0 - -30.0 °C
28.6 - 51.97 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 8.03 J/cm² Grade Count:51
Charpy Impact, Notched 1.00 - 6.09 J/cm²4.76 - 29.0 ft-lb/in²Average value: 2.09 J/cm² Grade Count:71
 1.00 - 4.60 J/cm²
@Temperature -30.0 - -30.0 °C
4.76 - 21.9 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.92 J/cm² Grade Count:50
Dart Drop, Total Energy  7.85 - 16.4 J
@Temperature -20.0 - -20.0 °C
5.79 - 12.1 ft-lb
@Temperature -4.00 - -4.00 °F
Average value: 12.1 J Grade Count:1
 7.85 - 16.4 J
@Thickness 3.18 - 3.18 mm
5.79 - 12.1 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 12.1 J Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cm1.00e+9 - 1.00e+16 ohm-cmAverage value: 2.06e+14 ohm-cm Grade Count:62
Surface Resistance 10000 - 1.00e+16 ohm10000 - 1.00e+16 ohmAverage value: 2.15e+14 ohm Grade Count:46
Dielectric Constant 3.80 - 6.403.80 - 6.40Average value: 4.50 Grade Count:4
Dielectric Strength 19.7 - 36.0 kV/mm500 - 914 kV/inAverage value: 29.2 kV/mm Grade Count:54
Dissipation Factor 0.0140 - 0.1690.0140 - 0.169Average value: 0.0530 Grade Count:4
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 590 V Grade Count:29
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 30.0 µm/m-°C5.56 - 16.7 µin/in-°FAverage value: 18.7 µm/m-°C Grade Count:45
CTE, linear, Transverse to Flow 30.6 - 90.0 µm/m-°C17.0 - 50.0 µin/in-°FAverage value: 55.3 µm/m-°C Grade Count:24
Thermal Conductivity 0.350 - 0.548 W/m-K2.43 - 3.80 BTU-in/hr-ft²-°FAverage value: 0.482 W/m-K Grade Count:3
Melting Point 220 - 325 °C428 - 617 °FAverage value: 263 °C Grade Count:51
Maximum Service Temperature, Air 100 - 270 °C212 - 518 °FAverage value: 171 °C Grade Count:27
Deflection Temperature at 0.46 MPa (66 psi) 220 - 260 °C428 - 500 °FAverage value: 252 °C Grade Count:24
Deflection Temperature at 1.8 MPa (264 psi) 210 - 300 °C410 - 572 °FAverage value: 251 °C Grade Count:83
Deflection Temperature at 8.0 MPa 175 - 250 °C347 - 482 °FAverage value: 210 °C Grade Count:26
Vicat Softening Point 240 - 255 °C464 - 491 °FAverage value: 250 °C Grade Count:4
Flammability, UL94 HBHBGrade Count:46
Glow Wire Test 650 - 700 °C1200 - 1290 °FAverage value: 658 °C Grade Count:5
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 315 °C158 - 599 °FAverage value: 199 °C Grade Count:9
Nozzle Temperature 92.8 - 325 °C199 - 617 °FAverage value: 270 °C Grade Count:7
Die Temperature 300 - 320 °C572 - 608 °FAverage value: 313 °C Grade Count:3
Melt Temperature 260 - 325 °C500 - 617 °FAverage value: 293 °C Grade Count:31
Mold Temperature 65.6 - 135 °C150 - 275 °FAverage value: 94.9 °C Grade Count:30
Drying Temperature 70.0 - 120 °C158 - 248 °FAverage value: 84.0 °C Grade Count:25
Moisture Content 0.0500 - 0.200 %0.0500 - 0.200 %Average value: 0.155 % Grade Count:14
Injection Pressure 3.45 - 150 MPa500 - 21800 psiAverage value: 67.2 MPa Grade Count:11
Vent Depth 0.00127 - 0.00254 cm0.000500 - 0.00100 inAverage value: 0.00148 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 50% Glass Fiber Filled
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Glass Fiber Filled
Overview of materials for Nylon 66, 20% Glass Fiber Filled

O2516 / 78015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.