MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Carbon Fiber Filled

Material Notes: Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS are added to the glass surface, endowing the product with multifunctional properties. This CNS-infused chopped glass product is designed for use as a reinforcement for thermoset and thermoplastic resins that not only yields enhanced mechanical properties, but also makes the material conductive.

Property data is for PC/ABS CNS-infused glass fiber 3%

Information provided by Applied Nanostructured Solutions (ANS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.150 g/cc0.00542 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiASTM D638
Tensile Modulus 8.96 GPa1300 ksiASTM D638
Flexural Strength 140 MPa20300 psiASTM D790
Flexural Modulus 8.76 GPa1270 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  35 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
35 dB
@Thickness 0.118 in,
Frequency 3.00e+7 Hz
15% glass; ASTM D4935
 40 dB
@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
40 dB
@Thickness 0.118 in,
Frequency 2.03e+9 Hz
15% glass; ASTM D4935
 44 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
44 dB
@Thickness 0.118 in,
Frequency 3.00e+7 Hz
25% glass; ASTM D4935
 50 dB
@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
50 dB
@Thickness 0.118 in,
Frequency 2.03e+9 Hz
25% glass; ASTM D4935
 51 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
51 dB
@Thickness 0.118 in,
Frequency 3.00e+7 Hz
30% glass; ASTM D4935
 60 dB
@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
60 dB
@Thickness 0.118 in,
Frequency 2.03e+9 Hz
30% glass; ASTM D4935
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 2.0 %<= 2.0 %
 
Descriptive Properties
% Sizing, type~5%Polyurethane
Chop Length6mm
Glass Tex850
Glass TypeE-CR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for PVC/Acrylic Alloy
Gold, Au
Iron, Fe
Silver, Ag

PANS001 / 176021

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.