MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Delrin Delrin® 100P NC010 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: High Viscosity Acetal Homopolymer with Improved Processing

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Melt Density 1.19 g/cc
@Temperature 215 °C
0.0430 lb/in³
@Temperature 419 °F
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
 1.4 %
@Thickness 2.00 mm
1.4 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.300 %
@Thickness 2.00 mm
0.300 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4, 2577
Melt Flow  2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ISO 2039-2
Hardness, Rockwell R 119119ISO 2039-2
Ball Indentation Hardness 173 MPa25100 psiH 358/30; ISO 2039-1
Tensile Strength, Yield 70.0 MPa10200 psiISO 527-1/-2
Elongation at Break 45 %45 %Nominal; ISO 527-1/-2
Elongation at Yield 26 %26 %ISO 527-1/-2
Tensile Modulus 2.90 GPa421 ksiISO 527-1/-2
Flexural Strength 75.0 MPa
@Strain 3.5 %
10900 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Poissons Ratio 0.370.37
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  40.0 J/cm²
@Temperature -30.0 °C
190 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2700 MPa392000 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1500 MPa218000 psi1000h; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance 2.00e+13 ohm2.00e+13 ohmIEC 62631-3-2
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 41.0 kV/mm1040 kV/inIEC 60243-1
Dissipation Factor  0.0035
@Frequency 100 Hz
0.0035
@Frequency 100 Hz
IEC 62631-2-1
 0.0055
@Frequency 1e+6 Hz
0.0055
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Specific Heat Capacity 3.00 J/g-°C
@Temperature 215 °C
0.717 BTU/lb-°F
@Temperature 419 °F
Melt
Thermal Conductivity 0.220 W/m-K
@Temperature 215 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 419 °F
Melt
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
 110 °C230 °FAnnealed; ISO 75-1/-2
Vicat Softening Point 160 °C320 °F50°C/h, 50N; ISO 306
 175 °C347 °F50°C/h 10N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 50.0 mm/min
@Thickness 1.00 mm
1.97 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 205 °C383 - 401 °FRange, Extrusion
 200 °C392 °FOptimum, Extrusion
 215 °C419 °FOptimum, Injection
 210 - 220 °C410 - 428 °FRange, Injection
Mold Temperature 90.0 °C194 °FOptimum, Injection
 80.0 - 100 °C176 - 212 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 80.0 °C176 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Extrusion
 <= 0.20 %<= 0.20 %Injection
Hold Pressure 90.0 - 110 MPa13100 - 16000 psiInjection
 110 MPa16000 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Emissions (mg/kg)<8VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOMISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100P BK602 POM
Delrin Delrin® 100 NC010 POM
Delrin Delrin® 500P NC010 POM
INEOS Styrolution Lustran® 348 Acrylonitrile Butadiene Styrene (ABS)
Delrin Delrin® 150 NC010 POM

PDSX5086 / 197726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.