MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Magnesium AZ91E-T6, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Magnesium AZ91A, B, C, D, and E have the same nominal composition but differ in ranges and/or specified impurity limits. This high purity alloy has excellent corrosion resistance. Commonly used in pressure-tight sand and permanent mold castings with high tensile strength and moderate yield strength. General purpose alloy, high strength.

Key Words: UNS M11919; Mg; European EN 1753 MC 21120; AMS 4446; ASTM B 94;SAE J465 (Ingot UNS M11918)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070500 kg load, 10 mm ball
Hardness, Knoop 9393Estimated from Brinell
Hardness, Rockwell E 7777
Hardness, Vickers 8080Estimated from Brinell
Tensile Strength, Ultimate 275 MPa39900 psi
Tensile Strength, Yield 145 MPa
@Strain 0.2 %
21000 psi
@Strain 0.2 %
Elongation at Break 6.0 %6.0 %in 50 mm
Tensile Modulus 44.8 GPa6500 ksi
Compressive Yield Strength 130 MPa18900 psiat 0.2% offset
Ultimate Bearing Strength 515 MPa74700 psi
Bearing Yield Strength 360 MPa52200 psi
Poissons Ratio 0.350.35
Fatigue Strength 85.0 MPa
@# of Cycles 5.00e+8
12300 psi
@# of Cycles 5.00e+8
R.R. Moore Test
Shear Modulus 17.0 GPa2470 ksi
Charpy Impact 1.40 J1.03 ft-lbV-Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000129 ohm-cm0.0000129 ohm-cm(AZ91C-T6)
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 373 J/g160 BTU/lb
CTE, linear  26.0 µm/m-°C
@Temperature 25.0 °C
14.4 µin/in-°F
@Temperature 77.0 °F
 27.2 µm/m-°C
@Temperature 20.0 - 200 °C
15.1 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 1.047 J/g-°C0.2502 BTU/lb-°F
Thermal Conductivity 72.7 W/m-K505 BTU-in/hr-ft²-°F
Melting Point >= 421 °C>= 790 °FIncipient Melting
Solidus 470 °C878 °F
Liquidus 595 °C1100 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 650 - 815 °C1200 - 1500 °FPermanent Mold Casting
 705 - 845 °C1300 - 1550 °FSand Casting
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.1 - 9.3 %8.1 - 9.3 %
Copper, Cu <= 0.015 %<= 0.015 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Magnesium, Mg 88.51 - 91.22 %88.51 - 91.22 %As Remainder
Manganese, Mn 0.17 - 0.35 %0.17 - 0.35 %
Nickel, Ni <= 0.0010 %<= 0.0010 %
Other, total <= 0.30 %<= 0.30 %
Silicon, Si <= 0.20 %<= 0.20 %
Zinc, Zn 0.40 - 1.0 %0.40 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AZ91E-T4, Cast
Magnesium AZ91E-F, Cast
Magnesium AZ91D-F, Cast
Magnesium AZ91C-T6, Cast
Magnesium AZ91A-F, Die Cast

MMAZ93 / 12339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.