MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is one of the High Productivity Nylon series products, offering the performance characteristics of a premium glass fiber reinforced polyamide while reducing cycle time and improving surface appearance. It is also available in heat stabilized (Capron HPN 9233G HS) and/or pigmented versions.

Capron HPN 9233G is generally recommended for high performance applications such as window locks, valve bodies, chair shells, door and window hardware, connectors, switch components, relay parts, terminal blocks, power tool housings, gears, chain saws, blowers, and trimmer housings.

Data provided by Allied Signal.

Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³(Dry)
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data MD (Dry)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 115 MPa16700 psiISO value at 5mm/min.
 120 MPa17400 psiASTM data at 5 mm/min.
Elongation at Break 5.0 %5.0 %ISO, 5 mm/min
 5.0 %5.0 %ASTM, 5 mm/min
Tensile Modulus 6.94 GPa1010 ksisame value from ASTM and ISO test.
Flexural Yield Strength 190 MPa27600 psiASTM Data
Flexural Modulus 6.12 GPa888 ksiASTM Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F(Dry)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 275 °C527 °FSee Materials Notes
Mold Temperature 95.0 °C203 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® GR630 30% Glass-Filled Nylon 66 (Dry)
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Conditioned)
Evonik Trogamid® T5002 Nylon 6-3 Compound
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)

PALD48 / 23942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.