MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastar GN120 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Appliances
  • Consumer electronics
  • Personal care and cosmetics
  • Stationary supplies

Key Attributes:

  • High clarity and transparency
  • High flow copolyester
  • Tough

Product Description: Eastar GN120 Copolyester is a high flow product and contains a mold release. Other outstanding features of Eastar GN120 are easily maintained such as excellent appearance and clarity, good physical properties, chemical resistance, and easy processing. Eastar GN120 is for sale only in Asia as a high-flow formulation.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength at Break 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 48.0 MPa6960 psiASTM D638
Elongation at Break 75 %75 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Flexural Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 1.90 GPa276 ksiASTM D790
Izod Impact, Notched  0.460 J/cm
@Temperature -40.0 °C
0.862 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.840 J/cm
@Temperature 23.0 °C
1.57 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy  35.0 J
@Temperature 23.0 °C
25.8 ft-lb
@Temperature 73.4 °F
At Max load; ASTM D3763
 44.0 J
@Temperature -40.0 °C
32.5 ft-lb
@Temperature -40.0 °F
At Max load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.40 %0.40 %ASTM D1003
Transmission, Visible 91 %91 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 71.0 °C160 °F
Dry Time 6 hour6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman DuraStar MN611 Polymer, Natural
Eastman DuraStar DS1910HF Polymer, Natural
BASF Ultrason® S 2010 PSU
BASF Ultrason® E 2010 PES
BASF Ultramid® C3U10 PA6/66 FR (Dry)

PE8811 / 129656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.