MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 556-LV Electrically & Thermally Conductive Material, Silver Filled
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Electrically Conductive, Silver-Filled Epoxy
Good Corrosion Resistance and Mechanical Strength to 340 ºF.
Paste and Low Viscosity Systems Available.

Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.90 g/cc
@Temperature 25.0 °C
2.90 g/cc
@Temperature 77.0 °F
mixed
Particle Size <= 20 µm<= 20 µm
Viscosity 4000 - 6000 cP4000 - 6000 cPMixed Viscosity at 25°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484
Shear Strength 7.58 MPa1100 psiTensile Shear
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00080 ohm-cm0.00080 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.20 W/m-K15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 171 °C340 °Fcontinuous
 191 °C375 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
Recommended Cure
 1440 min
@Temperature 22.2 °C
24.0 hour
@Temperature 72.0 °F
Alternative Cure
Pot Life 60.0 min
@Temperature 25.0 °C
60.0 min
@Temperature 77.0 °F
25 g
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorSilver
FillerSilver Flake
Mix Ratio by Weight100:4resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Ensolite™ ECF-400 EPDM crushed foam
A. Schulman ComAlloy E-16902N PPS Alloy, Electrically Conductive - Stainless Steel Fiber Filled
Armacell Ensolite™ EF0 EPDM crushed foam
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Asahi Kasei Stylac™ IC10N ABS Polymer, Electrically Conductive

PAREM18 / 24282

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.