MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethydco Advancene™ EE-4811-AAH High Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Blown film. A high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density successfully combine excellent performance at high extrusion rates with high film strength and rigidity. Tubular films of ADVANCENE™ EE-4811-AAH are recommended for high strength grocery sacks, shopping bags and notion and millinery bags. The excellent drawdown characteristic of this product permits production of high quality thin films for multiwall sack liners and replacements for thin paper products. The combination of strength and drawdown makes this resin ideal for downgauging in many applications. Films are readily treated and printed to give high quality graphics. It is compatible with color concentrates thus permitting the production of variety of colored films that serve as protective and attractive decorative wraps. Main Characteristics: hexene high density resin, high film strength, excellent drawdown.

Extrusion Notes: 2.5 in screw, grooved crew type, 1mm die cap, 215°C melt temp, 6lb/hr/in of die circumference output, 4in die diameter, 4 to 1 blow up ratio, 80 rpm screw speed, 30in frost line height.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
Thickness 12.7 microns0.500 mil
High Load Melt Index 11 g/10 min
@Load 21.6 kg,
Temperature 190 °C
11 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 27.6 MPa
@Thickness 0.0127 mm
4000 psi
@Thickness 0.000500 in
ASTM D882
Film Tensile Strength at Yield, TD 24.1 MPa
@Thickness 0.0127 mm
3500 psi
@Thickness 0.000500 in
ASTM D882
Film Elongation at Break, MD 270 %
@Thickness 0.0127 mm
270 %
@Thickness 0.000500 in
ASTM D882
Film Elongation at Break, TD 350 %
@Thickness 0.0127 mm
350 %
@Thickness 0.000500 in
ASTM D882
Flexural Modulus, 1% Secant 814 MPa118000 psiASTM D790B, ISO 178,
Puncture Energy 1.20 J0.885 ft-lbunivation method
Elmendorf Tear Strength MD 70 g
@Thickness 0.0127 mm
70 g
@Thickness 0.000500 in
method B; ASTM 1922, ISO 6383-2
Elmendorf Tear Strength TD 150 g150 gmethod B; ASTM 1922, ISO 6383-2
Dart Drop Test 150 g
@Thickness 0.0127 mm
0.331 lb
@Thickness 0.000500 in
ASTM 1709A, ISO 7765
Film Tensile Strength at Break, MD 55.2 MPa
@Thickness 0.0127 mm
8010 psi
@Thickness 0.000500 in
ASTM D882
Film Tensile Strength at Break, TD 53.8 MPa
@Thickness 0.0127 mm
7800 psi
@Thickness 0.000500 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FASTM D3418, ISO 3146
 216 °C421 °Fextrusion
Vicat Softening Point 124 °C255 °FASTM D1525, ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethydco Advancene™ bEE-4909-AAH High Density Polyethylene Resin
Ethydco Advancene™ EE-4010-AAH HDPE Pipe Extrusion
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
Ethydco Advancene™ EM-5420-AAH High Density Polyethylene Resin
Ethydco Advancene™ EM-5204-UVH High Density Polyethylene Resin

PETHYD906 / 200052

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.