MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP3000 High Temperature Protective Coating Inorganic, Metal Oxide Filled  (discontinued **)
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: For good corrosion, temperature and thermal shock resistance to 1300 ºF. This advanced material is specially formulated to adhere to steel and refractory products used in boilers, furnaces, kilns, stacks, and other high temperature structures. Benefits include extended equipment life, lower energy costs, and increased throughput.

Key Words: High Temperature Coatings
Vendors: Aremco’s Corr-Paint protective coatings are the most expansive line of ceramic, epoxy, silicone, and urethane based coatings for application from room temperature to 1500°F (816°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/cc
Solids Content 28.5 %28.5 %volume
 53.2 %53.2 %weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 600 - 1200 cP600 - 1200 cPMixed Viscosity
Thickness 25.4 microns1.00 milrecommended dry film thickness
 89.4 microns3.52 milestimated wet film thickness
Storage Temperature 4.44 - 29.4 °C40.0 - 85.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 704 °C1300 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hourTouch
 2.00 - 4.00 hour2.00 - 4.00 hourHandling
 1.00 - 24.0 hour1.00 - 24.0 hourRecoat
Cure Time  60.0 min
@Temperature 260 °C
1.00 hour
@Temperature 500 °F
>1 Hour Air Set Required Prior to Curing
 120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
>1 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
@Temperature 23.0 °C
6.00 Month
@Temperature 73.4 °F
 
Descriptive Properties
ColorLight Gray
Dry Film Coverage ft2/gal870at 1 mil
PrimerCP5000recommended for exterior applications in which salt fog or moisture are present
 Only Recommended for exterior applications in which salt fog or moisture are present
ThinnerCP3000-T

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Quartz-Coat™ 845-HV High Temperature Specialty Ceramic-Inorganic Coating
Aremco Quartz-Coat™ 845-D / 845-S High Temperature Specialty Coatings Inorganic, Silicon Filled
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxide Filled
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating

ZCAREM71 / 612

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.