MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics V-THERM™ Thermally Conductive Elastomer  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: V-THERM thermally conductive elastomer interface pads are designed for use between heat generating components and cooling devices. This material conforms to surface irregularities under moderate application pressures to fill air gaps between components and their heat sinks.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Deformation  10 %
@Thickness 1.52 mm,
Pressure 0.689 MPa
10 %
@Thickness 0.0600 in,
Pressure 100 psi
 12 %
@Thickness 1.02 mm,
Pressure 0.689 MPa
12 %
@Thickness 0.0400 in,
Pressure 100 psi
 16 %
@Thickness 1.02 mm,
Pressure 1.38 MPa
16 %
@Thickness 0.0400 in,
Pressure 200 psi
 16 %
@Thickness 1.52 mm,
Pressure 1.38 MPa
16 %
@Thickness 0.0600 in,
Pressure 200 psi
 48 %
@Thickness 1.02 mm,
Pressure 2.76 MPa
48 %
@Thickness 0.0400 in,
Pressure 400 psi
 49 %
@Thickness 1.52 mm,
Pressure 2.76 MPa
49 %
@Thickness 0.0600 in,
Pressure 400 psi
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Compression Set 80 %
@Temperature 125 °C,
Time 79200 sec
80 %
@Temperature 257 °F,
Time 22.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+14 ohm-cm4.00e+14 ohm-cmASTM D257
Dielectric Constant  2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
ASTM D150
 3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength 5.91 kV/mm150 kV/inASTM D149
Dissipation Factor  0.0013
@Frequency 100000 Hz
0.0013
@Frequency 100000 Hz
ASTM D150
 0.023
@Frequency 100 Hz
0.023
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  5.00 W/m-K
@Thickness 0.510 mm
34.7 BTU-in/hr-ft²-°F
@Thickness 0.0201 in
ASTM D5470
 6.00 W/m-K
@Thickness 1.02 mm
41.6 BTU-in/hr-ft²-°F
@Thickness 0.0402 in
ASTM D5470
 7.00 W/m-K
@Thickness 1.52 mm
48.6 BTU-in/hr-ft²-°F
@Thickness 0.0598 in
ASTM D5470
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Descriptive Properties
BinderSilicone
CarrierNone
ColorBlue
FillerBoron Nitride

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-THERM 1641 Thermally Conductive Silicone
Celanese CoolPoly® E5105 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate
Celanese CoolPoly® E4301 Thermally Conductive Polybutylene Terephthalate

PCHOME002 / 28224

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.