MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Quantum PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Water Absorption 0.030 %0.030 %ASTM D570
Water Absorption at Saturation 0.050 %0.050 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ASTM D785
Hardness, Rockwell R 8484ASTM D785
Hardness, Shore D 7777ASTM 2240
Tensile Strength 48.3 MPa7000 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Tensile Modulus 1.72 GPa250 ksiASTM D638
Flexural Strength 20.7 MPa3000 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Compressive Strength 72.4 MPa10500 psiASTM D695
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
Coefficient of Friction 0.580.58
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmASTM D257
Dielectric Constant 8.35
@Frequency 1e+6 Hz
8.35
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 63.0 kV/mm1600 kV/inASTM D149
Dissipation Factor 0.060
@Frequency 1e+6 Hz
0.060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 µm/m-°C66.0 µin/in-°FASTM D696
Thermal Conductivity 0.108 W/m-K0.750 BTU-in/hr-ft²-°FASTM C177
Melting Point 168 °C335 °FASTM D3417
Maximum Service Temperature, Air 138 °C280 °F
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omnia Plastica Kynar® PVDF
Manifattura Cattaneo PVDF
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber
ScanTube PVDF Tubing
Westlake Plastics Kynar® 740 PVDF Homopolymer

PQUANTU019 / 160443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.