MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical properties along with FDA compliance, TECAFORM AH ID is ideal for enhancing product safety in food processing applications.

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D790
Water Absorption 0.22 %
@Time 86400 sec
0.22 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.65 %0.65 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8686ASTM D785
Tensile Strength, Yield 64.0 MPa9280 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Tensile Modulus 2.80 GPa406 ksiASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.48 GPa360 ksiASTM D790
Compressive Strength 31.0 MPa4500 psiASTM D695
Izod Impact, Unnotched 0.534 J/cm1.00 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.210.2140 psi, 50 fpm; ASTM D3702
K (wear) Factor 131 x 10-8 mm³/N-M65.0 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm
Limiting Pressure Velocity 0.0507 MPa-m/sec1450 psi-ft/minASTM D792
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+12 ohm1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C61.0 µin/in-°FASTM D696
Melting Point 165 °C329 °FASTM D2133
Maximum Service Temperature, Air 100 °C212 °FContinuous; UL746B
 141 °C285 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Flammability, UL94 HBHBUL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Process Technologies Inc PTFE/Metal - Metal Detectable Sanitary Gasket
RTP Company ESD 303 EM Polycarbonate (PC), Glass Fiber - ESD Protection - Static Dissipative - Easy Molding
Delrin Delrin® 100 NC010 POM
Ensinger Delrin® 150 Homopolymer Acetal (POM)
RTP Company ESD 800 Acetal (POM), ESD Protection - Electrically Conductive

PENSIN058 / 104749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.