ELITE™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performance on automated packaging equipment. ELLITE™ 5400G resin complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2a. Information provided by Dow |