MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadium lighting and quartz vessels for the semiconductor industry. Standard viscosity is 200–400 cP; a higher viscosity coating, 845-HV, in the range of 500–800 cP is available upon request.

Key Words: High Temperature Coatings
Vendors: Aremco offers a wide range of ceramic, glass and silicone based coatings for ceramic, glass and quartz materials used in heater and lighting applications to 2000°F (1093°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/cc
Solids Content 22.9 %22.9 %by volume
 50.1 %50.1 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 200 - 400 cP200 - 400 cP
Thickness 25.4 microns1.00 milrecommended dry film thickness
 82.3 microns3.24 milestimated wet film thickness
Storage Temperature 12.8 - 29.4 °C55.0 - 85.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1090 °C2000 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Cure Time  5.00 min
@Temperature 482 °C
0.0833 hour
@Temperature 900 °F
Step 2
 10.0 min
@Temperature 93.3 °C
0.167 hour
@Temperature 200 °F
Step 1, preceded by >10 min. air set
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBrown-BlackCured
Dry Film Coverage ft2/gal495at 1 mil
Thinner845-T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating

CAREM37a / 138311

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.