MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5454-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95454; ISO AlMg3Mn; Aluminium 5454-O; AA5454-O; Al5454-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.69 g/cc0.0972 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6262AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 8585Converted from Brinell Hardness Value
Hardness, Vickers 7272Converted from Brinell Hardness Value
Tensile Strength, Ultimate 248 MPa36000 psiAA; Typical
 41.0 MPa
@Temperature 371 °C
5950 psi
@Temperature 700 °F
 75.0 MPa
@Temperature 316 °C
10900 psi
@Temperature 601 °F
 115 MPa
@Temperature 260 °C
16700 psi
@Temperature 500 °F
 150 MPa
@Temperature 204 °C
21800 psi
@Temperature 399 °F
 200 MPa
@Temperature 149 °C
29000 psi
@Temperature 300 °F
 250 MPa
@Temperature -28.0 °C
36300 psi
@Temperature -18.4 °F
 250 MPa
@Temperature 24.0 °C
36300 psi
@Temperature 75.2 °F
 250 MPa
@Temperature 100 °C
36300 psi
@Temperature 212 °F
 255 MPa
@Temperature -80.0 °C
37000 psi
@Temperature -112 °F
 370 MPa
@Temperature -196 °C
53700 psi
@Temperature -321 °F
Tensile Strength, Yield 117 MPa17000 psiAA; Typical
 29.0 MPa
@Temperature 371 °C
4210 psi
@Temperature 700 °F
 50.0 MPa
@Temperature 316 °C
7250 psi
@Temperature 601 °F
 75.0 MPa
@Temperature 260 °C
10900 psi
@Temperature 500 °F
 105 MPa
@Temperature 204 °C
15200 psi
@Temperature 399 °F
 110 MPa
@Temperature 149 °C
16000 psi
@Temperature 300 °F
 115 MPa
@Temperature -80.0 °C
16700 psi
@Temperature -112 °F
 115 MPa
@Temperature -28.0 °C
16700 psi
@Temperature -18.4 °F
 115 MPa
@Temperature 24.0 °C
16700 psi
@Temperature 75.2 °F
 115 MPa
@Temperature 100 °C
16700 psi
@Temperature 212 °F
 130 MPa
@Temperature -196 °C
18900 psi
@Temperature -321 °F
Elongation at Break  25 %
@Temperature 24.0 °C
25 %
@Temperature 75.2 °F
 27 %
@Temperature -28.0 °C
27 %
@Temperature -18.4 °F
 30 %
@Temperature -80.0 °C
30 %
@Temperature -112 °F
 31 %
@Temperature 100 °C
31 %
@Temperature 212 °F
 39 %
@Temperature -196 °C
39 %
@Temperature -321 °F
 50 %
@Temperature 149 °C
50 %
@Temperature 300 °F
 60 %
@Temperature 204 °C
60 %
@Temperature 399 °F
 80 %
@Temperature 260 °C
80 %
@Temperature 500 °F
 110 %
@Temperature 316 °C
110 %
@Temperature 601 °F
 130 %
@Temperature 371 °C
130 %
@Temperature 700 °F
 22 %
@Thickness 1.59 mm
22 %
@Thickness 0.0625 in
AA; Typical
Modulus of Elasticity 70.3 GPa10200 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Notched Tensile Strength 221 MPa32100 psi2.5 cm width x 0.16 cm thick side-notched specimen, Kt = 17.
Ultimate Bearing Strength 427 MPa61900 psiEdge distance/pin diameter = 2.0
Bearing Yield Strength 165 MPa23900 psiEdge distance/pin diameter = 2.0
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Fatigue Strength 120 MPa
@# of Cycles 5.00e+8
17400 psi
@# of Cycles 5.00e+8
unnotched R. R. Moore rotating beam
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 159 MPa23000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000515 ohm-cm
@Temperature 20.0 °C
0.00000515 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.9 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.2 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.7 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
 24.6 µm/m-°C
@Temperature 20.0 - 200 °C
13.7 µin/in-°F
@Temperature 68.0 - 392 °F
 25.6 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 134 W/m-K930 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 601.7 - 646.1 °C1115 - 1195 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 601.7 °C1115 °FAA; Typical
Liquidus 646.1 °C1195 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.4 - 97.1 %94.4 - 97.1 %As remainder
Chromium, Cr 0.05 - 0.20 %0.05 - 0.20 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.4 - 3.0 %2.4 - 3.0 %
Manganese, Mn 0.50 - 1.0 %0.50 - 1.0 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5083-O
Aluminum 5254-O
Aluminum 5454-H32
Aluminum 5454-H111; 5454-H311
Aluminum 5052-O

MA5454O / 9281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.