Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing with another typical LLDPE. It processing aid and antioxidant additives. Applications: Heavy-duty bags; Liners; LDPE and HDPE blends; Packages for general use. Additives: PPA Information provided by Braskem. |