MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description

POLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. POLYBATCH® B8750A has also been formulated with an antistatic agent to provide dust control in the finished part. POLYBATCH® B8750A is recommended for use at 2 to 5% addition levels.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
Bulk Density 0.900 g/cc0.0325 lb/in³
Moisture Absorption <= 0.150 %<= 0.150 %ASTM D789
Additive Loading 4.8 %4.8 %
Ash 50 %50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin
Armacell Ensolite™ IG1 PVC/NBR/CR

PASHU497 / 25461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.