MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® BZM 30 BLACK TL Nylon 11, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 with 30% Glass Fiber Filler

Material Notes: Designation ISO 1874-PA11,MHL,18-050,GF30

Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.

Rigidity. High compressive strength. Low linear expansion coefficient. Low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability.

UL classification: UL94 HB RTI(C) 65/65/65

Example applications: Wind turbine, casing.

Information provided by Arkema.

Key Words: PA11; Polyamide 11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
 1.25 g/cc0.0452 lb/in³Cond.; ISO 1183
Water Absorption 1.3 %1.3 %Dry; Sim. to ISO 62
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 235 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 74
@Time 15.0 sec
74
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 110 MPa16000 psiCond.; ISO 527-1/-2
Elongation at Break 6.0 %6.0 %Cond.; ISO 527-1/-2
Tensile Modulus 6.90 GPa1000 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  7.40 J/cm²
@Temperature 23.0 °C
35.2 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
 8.30 J/cm²
@Temperature -30.0 °C
39.5 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 189 °C372 °F10°C/min; Dry; ISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Hold Pressure 22.0 MPa3190 psiInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based95ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® BZM 30 O TL PA11-GF30
Celanese Celstran® PP-GF30-03-Black PP, 30% Glass Reinforced
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned)
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® MB 3000 NAT Nylon 11, Sheathing Grade

PARKG646 / 25898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.