MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0055 cm/cm0.0035 - 0.0055 in/in
Linear Mold Shrinkage, Transverse 0.0065 - 0.0090 cm/cm0.0065 - 0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  65.0 MPa
@Temperature 150 °C
9430 psi
@Temperature 302 °F
 75.0 MPa
@Temperature 120 °C
10900 psi
@Temperature 248 °F
 80.0 MPa
@Temperature 90.0 °C
11600 psi
@Temperature 194 °F
 105 MPa
@Temperature 60.0 °C
15200 psi
@Temperature 140 °F
 145 MPa
@Temperature 23.0 °C
21000 psi
@Temperature 73.4 °F
Elongation at Break  3.2 %
@Temperature 23.0 °C
3.2 %
@Temperature 73.4 °F
 4.6 %
@Temperature 60.0 °C
4.6 %
@Temperature 140 °F
 6.7 %
@Temperature 90.0 °C
6.7 %
@Temperature 194 °F
 7.6 %
@Temperature 120 °C
7.6 %
@Temperature 248 °F
 8.6 %
@Temperature 150 °C
8.6 %
@Temperature 302 °F
Tensile Modulus  3.40 GPa
@Temperature 150 °C
493 ksi
@Temperature 302 °F
 3.80 GPa
@Temperature 120 °C
551 ksi
@Temperature 248 °F
 4.60 GPa
@Temperature 90.0 °C
667 ksi
@Temperature 194 °F
 7.50 GPa
@Temperature 60.0 °C
1090 ksi
@Temperature 140 °F
 10.5 GPa
@Temperature 23.0 °C
1520 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °F
Vicat Softening Point 215 °C
@Load 5.00 kg
419 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Oxygen Index 32 %32 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature  755 °C
@Thickness 2.00 mm
1390 °F
@Thickness 0.0787 in
 775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant

PLATH9689 / 177385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.