MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher toughness and faster production rates than traditional composite materials. The technology, using ISOPLAST® Engineering Thermoplastic Polyurethane (ETPU), allows production of hollow as well as solid elongated profiles using pultrusion techniques.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.86 g/cc0.0672 lb/in³ASTM D792
Filler Content 66 %66 %Glass
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 1050 MPa152000 psiASTM D4476
Flexural Modulus 40.0 GPa5800 ksiASTM D4476
Compressive Strain at Break 1.5 %1.5 %ASTM D695
Compressive Strength 440 MPa63800 psiASTM D695
Compressive Modulus 35.0 GPa5080 ksiASTM D695
Shear Strength 55.0 MPa7980 psiASTM D3846
Izod Impact, Notched 41.0 J/cm76.8 ft-lb/inASTM D256
Izod Impact, Unnotched 59.0 J/cm111 ft-lb/in3 strips glued together; ASTM D4812

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® PF-1000 Polysulfone
Evonik VESTANAT® TMDI Diisocyanate
Gharda Chemicals GAFONE™-S 20% Glass Fiber-Reinforced PSU, High Thermal Stability
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Overview of materials for Polycarbonate, Extruded

PDWFUL01 / 34615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.