MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9868DU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes:
  • injection molding grade
  • very good hydrolysis and microbial resistance
  • very good low-temperature impact strength
  • opaque
  • Cylindrical pellets
Application
  • Boot shells
  • Technical parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ISO 868
Hardness, Shore D 6565ISO 868
Tensile Strength, Ultimate 52.0 MPa7540 psi200 mm/min; DIN 53504
Tensile Stress at Strain  21.0 MPa
@Strain 10 %
3050 psi
@Strain 10 %
200 mm/min; DIN 53504
 25.0 MPa
@Strain 50 %
3630 psi
@Strain 50 %
200 mm/min; DIN 53504
 28.0 MPa
@Strain 100 %
4060 psi
@Strain 100 %
200 mm/min; DIN 53504
 43.0 MPa
@Strain 300 %
6240 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 367 %367 %200 mm/min; DIN 53504
Tensile Modulus  0.268 GPa
@Temperature 60.0 °C
38.9 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.684 GPa
@Temperature 20.0 °C
99.2 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 1.20 GPa
@Temperature -20.0 °C
174 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Flexural Modulus 0.548 GPa79.5 ksi2 mm/min; ISO 178
Rebound 53 %53 %Resilience; ISO 4662
Tear Strength 160 kN/m913 pli500 mm/min; ISO 34-1
Abrasion 3737mm³, Method A; ISO 4649
Compression Set  48 %
@Temperature 23.0 °C
48 %
@Temperature 73.4 °F
72 hr; ISO 815
 55 %
@Temperature 70.0 °C
55 %
@Temperature 158 °F
24 hr; ISO 815
 32 %
@Temperature 70.0 °C,
Time 86400 sec
32 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 235 °C437 - 455 °FInjection
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 9864DU TPU
Covestro Desmopan® 9395AU Polyurethane
Covestro Desmopan® 85786A Polyurethane
Covestro Desmopan® 9095AU Polyurethane
Covestro Desmopan® 9386A Polyurethane

PB09823 / 92663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.