MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical SBR 1500H High Acrylonitrile Polymer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: SBR 1500H is a cold polymerized styrene-butadiene copolymer with non-staining stabilizer and especially well-suited for adhesive applications. It has high internal strength, and excellent shear and peel adhesion. And also SBR 1500H has good processability, high solubility in solvent and no gel characteristic.

Applications: SBR 1500H can be used to conveyor belt and hand-built hose where good building tack and light color are required

CAS No: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/cc
Volatiles 0.30 %0.30 %
Mooney Viscosity 52
@Temperature 100 °C
52
@Temperature 212 °F
ML 1+4
Ash 0.20 %0.20 %
 
Chemical PropertiesMetricEnglishComments
Styrene Content 23.5 %23.5 %Bound
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.4 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
4120 psi
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
Elongation at Break 520 %
@Treatment Temp. 145 °C,
Time 2100 sec
520 %
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
300% Modulus 15.7 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
2280 psi
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
 
Descriptive Properties
ColorLight Tan Bale
ComponentsHAF50, ASTM D3185
 SBR 1500H100, ASTM D3185
 Stearic Acid1, ASTM D3185
 Sulfur1.75, ASTM D3185
 TBBS1, ASTM D3185
 ZnO3, ASTM D3185
Organic Acid6.1%
Soap0.1%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer
Lucobit Lucopren® 1500H Soft Polyolefin Granules
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Garlock Super Rinohide™ 7160 SBR Rubber Lining
Garlock 7164 SBR Rubber Lining

PLAY744 / 148754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.