MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock 7164 SBR Rubber Lining
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR rubber lining for protection applications such as chute lining and skirtboards.

An optional duck fabric backing is available.

Information provided by Garlock Rubber Technologies

Key Words: ASTM D2000-BA-620
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65
Tensile Strength >= 13.8 MPa>= 2000 psi
 16.5 MPa2400 psiTypical
Elongation at Break >= 300 %>= 300 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF D 2000 Polyetheramine
Garlock 244 Neoprene Rubber - Commercial Grade
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Rubatex R421 Neoprene/EPDM/SBR Rubber Foam Sheet
LG Chemical SBR 1500H High Acrylonitrile Polymer

PGARL982 / 157455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.